Hello,
I've been having some issues with making fine leather. So far I've used 160l of 50% rose-tinted tanning fluid but only got 8 fine leather (and 8 normal leather). I was under the assumption that 10l of 50% rose-tinted tanning fluid was meant to be a guaranteed fine leather so can anyone show me what I'm doing wrong?
Here is how I make fine leather:
1. put 1l of otto rose into 10l vegetable oil
2. make limed hide
3. put limed hide and 50% rose-tinted tanning fluid in tub and wait 8 hours
4. only achieve 50% success qq
So is it only meant to be a 50% chance or am I doing something wrong?